Success Story: A Novel Approach to Estimate the Transition temperature via Dynamic Nanoindentation

In Hylley, we developed a material-efficient low-temperature nanoindentation method to assess temperature-dependent deformation behavior and estimate transition temperatures associated with the ductile-to-brittle transition. Only a single small specimen is required.

 

Success Story DBTT

 

Funding

We would like to thank: